Sintered Samarium Cobalt Magnets, SmCo Magnet

  • Price:

    Negotiable

  • minimum:

  • Total supply:

  • Delivery term:

    The date of payment from buyers deliver within days

  • seat:

    Hunan

  • Validity to:

    Long-term effective

  • Last update:

    2017-12-19 16:41

  • Browse the number:

    296

Send an inquiries

Company Profile

Ganzhou Wanfeng Advanced Materials Technology Co., Ltd.

By certification [File Integrity]

Contact:Mr. Richard Liu(Mr.)  

Email:

Telephone:

Phone:

Area:Hunan

Address:Hunan

Website: http://summitmagnet.huasengtex.com/

Product details
SmCo Rare Earth Magnets Overview

Two common compositions of SmCo magnets are Sm1Co5 and Sm2Co17. Generally, the cost of SmCo magnets is higher than NdFeB magnets. As a big advantage, SmCo magnets can operate at higher temperatures up to 300 degrees Centigrade. SmCo magnets are widely used in applications in which higher operating temperature and higher corrosion and oxidation resistance are crucial. The main ingredient of SmCo permanent magnet is metal cobalt(CoY99.95%). So its price is high!


SmCo Rare Earth Magnets Properties

Materials Grade Br (Residual induction) Hcb (Coercive Force) Hcj (Intrinsic coercive Force) (BH)max. Max. Energy Product Max. Operating Temp. TC
Curie Temp.


(KGs) (KOe) (KOe) (MGOe) (°c) (°c)
Sm1Co5 YX-16 8.1-8.5 7.8-8.3 15-23 14-16 250 750
Sm1Co5 YX-18 8.5-9.0 8.3-8.8 15-23 16-18 250 750
Sm1Co5 YX-20 9.0-9.4 8.5-9.1 15-23 19-21 250 750
Sm1Co5 YX-22 9.2-9.6 8.9-9.4 15-23 20-22 250 750
Sm1Co5 YX-24 9.6-10 9.2-9.7 15-23 22-24 250 750
Sm1Co5 YX-18s 8.5-9 8.3-8.8 18-25 17-19 250 750
Sm1Co5 YX-20s 9.0-9.4 8.5-9.1 18-25 18-20 250 750
Sm1Co5 YX-22s 9.2-9.6 8.9-9.4 18-25 20-22 250 750
Sm1Co5 LTc(YX-10) 5.9-6.3 5.8-6.2 18-23 8.5-10 250 700
Sm2Co17 YXG-24H 9.5-10.2 8.7-9.4 ≥25 22-24 350 800
Sm2Co17 YXG-26H 10.2-10.5 9.4-9.8 ≥25 24-26 350 800
Sm2Co17 YXG-28H 10.3-10.8 9.5-10 ≥25 26-28 350 800
Sm2Co17 YXG-30H 10.8-11.0 9.9-10.5 ≥25 28-30 350 800
Sm2Co17 YXG-22 9.3-9.7 8.5-9.3 ≥18 20-23 300 800
Sm2Co17 YXG-24 9.5-10.2 8.7-9.4 ≥18 22-24 300 800
Sm2Co17 YXG-26 10.2-10.5 9.4-9.8 ≥18 24-26 300 800
Sm2Co17 YXG-28 10.3--10.8 9.5-10 ≥18 26-28 300 800
Sm2Co17 YXG-30 10.8-11.0 9.9-10.5 ≥25 28-30 300 800
Sm2Co17 YXG-32 11-11.3 10.2-10.6 ≥15 29-32 300 800
Sm2Co17 YXG-26M 10.2-10.5 9.4-9.8 12-16 24-26 300 800
Sm2Co17 YXG-28M 10.3-10.8 9.5-10 12-16 26-28 300 800
Sm2Co17 YXG-30M 10.8-11.0 9.9-10.5 12-16 28-30 300 800
Sm2Co17 YXG-32M 10.8-11.0 9.9-10.5 12-16 29-32 300 800
Sm2Co17 YXG-28L 10.2-10.8 5.2-9.0 5.5-10 26-28 250 800
Sm2Co17 YXG-30L 10.8-11.5 5.2-9.0 5.5-10.0 28-30 250 800
Sm2Co17 YXG-32L 11-11.3 5.2-9.0 5.5-10.0 29-32 250 800
Sm2Co17 LTC(YXG-22) 9.4-9.8 8.4-9.0 15-20 21-23 300 840

Physical Characteristics

Sm1Co5 Sm2Co17
Temperature Coefficient of Br (%/°C) -0.05 -0.03
Temperature Coefficient of iHc (%/°C) -0.3 -0.2
Curie Temperature (°C) 700-750 800-850
Density (g/cm3) 8.2-8.4 8.3-8.5
Vickers Hardness (HV) 450-500 500-600
Working Temperature (°CC) 250 350



Key Advantages

SmCo magnets can operate at higher temperatures up to 300 degrees Centigrade.
High magnetic performance - up to about 32MGOe.
No need to be protected against oxidation.
Quick Leads

Density - 8.3 g/ cm³ (Sm1Co5), 8.4 g/ cm³ (Sm2Co17)
Manufacturing process - sintering (most common), with some injection molding and compression bonding.
Various shapes-- blocks, bars, discs, rings, arc segments, cylinders, etc.
Wide range of Grades - from about 1410 to 3214. (First 2 digits represent BH.max, and second two digits represent Intrinsic Coercivity, Hci.)
High magnetic performance - up to about 32MGOe.
Saturation magnetizing field required - about 50kOe
Operate at higher temperatures up to 300°c.

Common Applications